NMC Application Test of Mechanical Strength Improvement

NMC Application Test of Mechanical Strength Improvement

分享到

Wintern ecoTech Co., Ltd.

NMC Application Test of Mechanical Strength Improvement

Add to NMC 0.08%  Film Thickness reduction 20%

 

12u PE Film add to NMC Master Batch 3% vs Metallocene 30%

 

NMC enhance the physical properties of EPE materials

 

 

 

LCP Regrind materials +NMC Modifier

 

 

LCP 60% of the regrind material + NMC test compliance with RoHS

 

 

Food container PP cups add NMC to increase toughness & strength

 

SGS plastic food containers pass FDA test